Model No.
|
96178
|
Temperature Range
|
0°C to 1000°C
|
Resistance Value
|
Ro = 0.25Ω (others to special request)
|
Resistance Ratio
|
Wga>1.11807
|
Dimensions
|
Length 650mm
Diameter 7.5mm
|
Drift during use
|
|
a. Smallest
|
When taken to 970°C slowly over 1 to 2 hours and cooled slowly again (overnight) to 450°C, the triple point of water resistance will repeat to better than a temperature equivalent of 0.0005°C
|
b. Largest
|
When thermally shocked from 970°C to 20°C the triple point of water resistance will increase by a temperature-equivalent of up to 35mK; this is mostly recoverable upon annealing at 650°C for a few hours and then cooling slowly (overnight) to 450°C
|
Long term drift
|
Most changes occur during heating and cooling. If this process is done carefully, long term stabilities of a few mK per year can be expected, with reproducibility at the silver point of 3 to 5 mK.
|
State "with UKAS calibration" or "without UKAS calibration".
Refer to introduction for Calibration Uncertainties.